ChevronTexaco Clarity® ISO 100 Saw Guide Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Clarity®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Clarity® ISO 100 Saw Guide Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Clarity Saw Guide Oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.Chevron Clarity Saw Guide Oils are formulated with ISOSYN® base stocks and specially selected ashless additives to reduce friction between saw and guide components in thin kerf saw equipment.The oils lubricity performance minimizes rust and corrosion problems, while reducing friction to allow much cooler operation.Chevron Clarity Saw Guide Oils have been formulated with effective rust inhibitors to prevent rust formation. Oiliness and EP properties provide excellent film strength for boundary lubrication and extreme pressure conditions.Chevron Clarity Saw Guide Oils have the optimum emulsification to allow the correct mixing of oil and water and have tackiness properties to enable the lubricants to cling to saw and guide components.ApplicationsChevron Clarity Saw Guide Oils are specifically formulated to lubricate modern thin kerf sawing systems. Original Equipment Manufacturers and sawmill customers were consulted prior to product design and laboratory testing. Chevron Clarity Saw Guide Oils performance properties have been field proven to meet the severe requirements of this application.Chevron Clarity Saw Guide Oils meet or exceed the performance requirements of most saw system manufacturers, including: CAE (Newnes, McGehee), Optimil, Salem, TMT, Ukiah, and USNR (Kockums CanCar, Schurman). Chevron Clarity Saw Guide Oil ISO 46 is recommended for and has been used successfully in band saw mist applications.
Physical Properties Metric English Comments
API Gravity 31.7 °
31.7 °
Viscosity Measurement 105
105
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 494 SUS
494 SUS
Saybolt Viscosity at 210°F 65 SUS
65 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
95 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11.3 cSt
11.3 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -33.0 °C
-27.4 °F
ASTM D97
Flash Point 262 °C
504 °F
ASTM D92
Descriptive Properties Value Comments
Rust preventative Test Procedure B Pass
Synthetic Sea Water