Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil 10W Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 1000 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 150 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 320 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 460 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | <= -33.0 °C | <= -27.4 °F | ASTM D97 |
ExxonMobil 320 Mobil SHC PM Series Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex.. |
|||
Pour Point | -33.0 °C | -27.4 °F | |
ChevronTexaco 32 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco Delo® 100 Motor Oil, SAE 20 Chevron Delo 100 Motor Oils are high performance crankcase oils for diesel engines.They are manufactured using selected premium paraffinic base oils and detergent, dispersant, wear control, antioxid.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco Delo® 400 SAE 40 Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco HD Soluble Oil FeaturesChevron Soluble Oils are used broadly in machine shops as multifunctional cutting fluids. They are primarily designed to cool and lubricate the contact point of the tool and the work piece.C.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco ISO 32 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco ISO 46 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Pour Point | -33.0 °C | -27.4 °F | |
ChevronTexaco Starguide™ ISO 46 Texaco Starguide oils deliver value through:Cleaner cutting — Reduce excessive drag that slows cutting.Exceptional performance for low water and low oil consumption saw systems.Excellent low temper.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco Supreme SAE 5W-20 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil 10W Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil 15W-40 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 1000 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 460 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 680 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Vactra 2 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Zerice 32 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco Clarity® ISO 100 Saw Guide Oil FeaturesChevron Clarity Saw Guide Oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.Chevro.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco Delo® 300 Motor Oil, SAE 30 Features:Chevron Delo 300 Motor Oils are high sulfated ash superior “Series 3-type” crankcase oils for four-stroke diesel engines requiring a high detergent crankcase oilThey are manufactured usin.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco GST® ISO 68 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco RPM® SAE 80W-90 Universal Gear Lubricant FeaturesChevron RPM Universal Gear Lubricants are multipurpose lubricants.They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protecti.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Glygoyle 150 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ExxonMobil Mobil Vactra 2 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Pour Point | -33.0 °C | -27.4 °F | |
ChevronTexaco Havoline® SAE 5W-20 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |
|||
Pour Point | -33.0 °C | -27.4 °F | ASTM D97 |
ChevronTexaco Regal® 32 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Pour Point | -33.0 °C | -27.4 °F | |
ChevronTexaco Havoline® SAE 30 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |