ChevronTexaco Clarity® ISO 100 Synthetic Paper Machine Oil

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer ChevronTexaco Corp
Trade Name Clarity®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Clarity® ISO 100 Synthetic Paper Machine Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) synthetic base oils. This combination provides greatly enhanced thermal and oxidation stability.In addition, the high viscosity index of PAO base oils offers greater lubricant film thickness than the mineral oil-based products at high operation temperatures.The synthetic versions of Chevron Clarity Paper Machine Oils also offer better EP properties, allowing them to be used as EP gear lubricants.Chevron Clarity Synthetic Paper Machine Oils have excellent demusability (water separating ability) and wet filterability, as defined by the Pall Filterability Test.Chevron Clarity Synthetic Paper Machine Oils can be combined with mineral oil products for recycling purposes. They are fully compatible with the mineral oils products, Chevron Clarity Paper Machine Oils.They provide longer lubricant life due to superior oxidation stability, resulting in less lubricant usage, and reduced disposal.Chevron Clarity Synthetic Paper Machine Oils pass the LC 50 aquatic toxicity test.ApplicationsChevron Clarity Synthetic Paper Machine Oils may be used in the following applications:Extreme temperature bearing and circulation oil systemsGear boxesDryer section accessoriesMoisture profilerCalendar rollsCrown control rollsOil heated rollsHigh temperature air compressorsHigh pressure hydraulic pumpsDo not use in high pressure systems in the vicinity of flames, sparks, and hot surfaces. Use only in well ventilated areas. Keep container closed.
Physical Properties Metric English Comments
API Gravity 37.4 °
37.4 °
Viscosity Measurement 157
157
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 485 SUS
485 SUS
Saybolt Viscosity at 210°F 77 SUS
77 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
95 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
Oxidative Stability >= 8000 hour
>= 8000 hour
Mechanical Properties Metric English Comments
Timken Test 29500 g
65.0 lb
Thermal Properties Metric English Comments
Pour Point -48.0 °C
-54.4 °F
ASTM D97
Flash Point 264 °C
507 °F
ASTM D92
Descriptive Properties Value Comments
FZG Gear Wear Test, Failure Load Stage 13
Pall Filterability, Wet aged, mL to 25 psi >10000