ChevronTexaco Havoline® SAE 5W-30 Synthetic Motor Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Havoline®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Havoline® SAE 5W-30 Synthetic Motor Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Havoline Synthetic Motor Oil is recommended for all four-stroke gasoline engines used in passenger cars, sport utility vehicles, and light trucks. 5W-30 and 10W-30 meet: API Service Categories SL/CF, SJ/CF, SH, SG, Energy conserving for API SLILSAC GF-3ACEA A1-98General Motors GM 9986125, 9986126, 9986137, 4718MChrysler MS 6395-HFord ESE-M2C 153-GJapanese VTWPeugeot TU 3M Scuff TestDepartment of Defense Commercial Item Description A-A-52309BTypical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222102; MSDS Number: 8602
Physical Properties Metric English Comments
API Gravity 31.7 °
31.7 °
Viscosity 3700 cP

@Temperature -30.0 °C
3700 cP

@Temperature -22.0 °F
Cold Crank
Viscosity Measurement 172
172
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 58.1 cSt
58.1 cSt
Kinematic Viscosity at 100°C (212°F) 10.5 cSt
10.5 cSt
Ash 0.93 %
0.93 %
Sulfated Ash
Thermal Properties Metric English Comments
Pour Point -42.0 °C
-43.6 °F
Flash Point 244 °C
471 °F
Component Elements Properties Metric English Comments
Phosphorous, P 0.098 %
0.098 %
Zinc, Zn 0.107 %
0.107 %
Chemical Properties Metric English Comments
Total Base Number 8.6
8.6
ASTM D2896
Descriptive Properties Value Comments
Noack Volatility, wt% 10
250°C, 1 h