ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured using selected highly refined high viscosity index base oils, a lithium complex soap, a 3% molybdenum disulfide ("moly") antiwear agent, plus oxidation and rust inhibitors. They are dark gray in color and buttery in texture.Chevron RPM Heavy Duty LC Greases EP are available in two grades:NLGI 1 for better pumpability at low ambient temperaturesNLGI 2 for normal ambient temperaturesApplicationsChevron RPM Heavy Duty LC Greases EP are recommended as multipurpose products for the lubrication of both over-the-road and off-highway trucks, tractors, and heavy duty equipment. They give excellent performance in all automotive equipment in severe service.They provide top protection to fifth wheels, king pins, wheel bearings, steering system bearings, and all chassis points including ball joints and universal joints. They also perform well in most heavy duty industrial applications for general lubrication and for the lubrication of journal bearings, and low and moderate speed antifriction bearings.They are particularly effective in applications where a high dropping point and high EP are desirable. They perform well under high temperature, wet, and dusty operating conditions.Chevron RPM Heavy Duty LC Greases EP are registered with NSF and are acceptable as lubricants where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.
Physical Properties Metric English Comments
Viscosity Measurement 90
90
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 914 SUS
914 SUS
Saybolt Viscosity at 210°F 82 SUS
82 SUS
Kinematic Viscosity at 40°C (104°F) 173 cSt
173 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 15.5 cSt
15.5 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Weld Point
Four Ball Wear 0.500 mm
0.0197 in
Penetration 325
325
Worked
Penetration P(0), 1/10 mm 285
285
Timken Test 18100 g
40.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 198 °C
388 °F
ASTM D92
Dropping Point 260 °C
500 °F
Descriptive Properties Value Comments
Color Dark Gray/Black
Texture Smooth, Buttery
Thickener, % / type 9 / Lithium Complex