Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
Precision Polymer Engineering V72H Fluoroelastomer Compound Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admi.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z75G Hydrogenated NBR Compound Green Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5... |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z75R Hydrogenated NBR Compound Red Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5.Ap.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z90B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR. To meet ASTM D2000 line call-out M2DH920, A26, B16, EO16, EO36, F14.Ap.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Gehman T100 |
Zeon Chemicals HyTemp® 4451CG AR Polyacrylate Elastomer HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Particulate version of HyT.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
Chesterton 613 Moly Grease Description: Chesterton® 613 Moly Grease is a high-performance, cost-effective lubricant that can withstand extreme temperatures and pressures for a wide range of high and low-speed applications. F.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Crater® Fluid H Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco Delo® NLGI 1 Grease EP FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Molytex® EP NLGI Grade 2 Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle .. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
ChevronTexaco RPM® NLGI 2 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-751 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent metal bonding and compression set.Infor.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | TR test, TR10 |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4714 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM019602 MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM05540K MC Polyester Label Products 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 3302 Specialty Foil Tape Aluminum foil tape. EMI/RFI shielding. Ul 510 Recognized.Information provided by 3M |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 3325 Copper Foil Tape EMI/RFI shielding. UL 510 Recognized.Information provided by 3M |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM0196J MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FV1002 Soft White Vinyl EDP Label Product 3M™ Soft White Vinyl EDP Label Products FV100K and FV1002 are flexible vinyl label stocks that offer excellent durability and some moisture resistance. These vinyl labels utilize 3M™ Adhesive F220.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M Scotch® Super 88 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape Super 88 is a premium grade, 8.5 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 3513 Copper Foil Tape EMI/RFI shielding. UL 510 Recognized.Information provided by 3M |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | |
3M 4726 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M 8067 All Weather Flashing Tape 3M™ All Weather Flashing Tape 8067 is a self-adhered, waterproof flashing membrane designed for sealing around openings and penetrations in exterior walls. This product has a unique acrylic pressur.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | Application |
3M FM01961K MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Minimum Service Temperature, Air | -18.0 °C | -0.400 °F | See Note 1. |
ChevronTexaco Crater® CSF Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |