Material Notes:
FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined, select high viscosity index base oils, and a lithium complex soap. It is red in color and smooth and stringy in texture. Chevron RPM Automotive LC Grease EP NLGI 2 is for use in normal ambient temperaturesApplicationsChevron RPM Automotive LC Grease EP is recommended for:general use in the lubrication of trucks, tractors, and passenger cars. This includes ball joints, universal joints, and all other chassis points, wheel bearings, water pumps, and fifth wheels. boat trailer wheel bearingshigh temperature disc brake bearing applicationsIt is approved for the NLGI Certification Mark GC-LB. Chevron RPM Automotive LC Grease EP is registered with NSF and is acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.
Physical Properties Metric English Comments
Viscosity Measurement 90
90
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 914 SUS
914 SUS
Saybolt Viscosity at 210°F 82 SUS
82 SUS
Kinematic Viscosity at 40°C (104°F) 173 cSt
173 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 15.5 cSt
15.5 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Weld Point
Four Ball Wear 0.500 mm
0.0197 in
Penetration 280
280
Worked
Penetration P(0), 1/10 mm 267
267
Timken Test 18100 g
40.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 198 °C
388 °F
ASTM D92
Dropping Point 270 °C
518 °F
Descriptive Properties Value Comments
Color Dark Green
Texture Smooth, Buttery
Thickener, % / type 12 / Lithium Complex