ChevronTexaco URSA® SAE 40 Premium TDX

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name URSA®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco URSA® SAE 40 Premium TDX.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Ursa Premium TDX delivers value through:Reduced wear — Prolonging component life and providing reduced maintenance costs.Improved engine cleanliness — Providing efficient operation and reduced fuel consumption.Extended drain capability — Reducing operating costs (approved by Mack, Cummins, Mercedes Benz, MTU, MAN).Oil consumption control — Controls wear and piston deposits resulting in reduced emissions.Engine durability even under arduous extended oil drain periods.Texaco Ursa Premium TDX is a super high performance diesel engine oil (SHPD) specially designed for use in heavy duty turbocharged diesel engines with extended drain interval approval for various engine manufacturers.Texaco Ursa Premium TDX, SAE 30 and 40, is recommended for four-stroke naturally aspirated, turbocharged, and supercharged diesel engines in all types of service.It is ideal for mixed commercial fleets, farm machinery, construction equipment, marine and other off-highway applications.It can also be used in four-stroke gasoline engines. Texaco Ursa Premium TDX, SAE 30 and 40, meets:API Service CategoriesCF, CD1SL, SJ, SH, SG1Major diesel engine manufacturers requirementsMTU/DDC Category 1MAN M270Mercedes Benz 228.1Volvo VDSPerformance requirements ofAllison C4 Fluids (SAE 30)Caterpillar TO-2 (SAE 30)Manufacturers performance requirementsGeneral Motors GM 6094-MDepartment of Defense Commercial Item Description (CID)A-A-52306A22Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Obsolete Specification.Engine performance equivalent to MIL-PRF-2104G, MIL-L-46152E.CPS Number: 222155; MSDS Number: 8603
Physical Properties Metric English Comments
API Gravity 28.9 °
28.9 °
Viscosity Measurement 102
102
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 146 cSt
146 cSt
Kinematic Viscosity at 100°C (212°F) 14.9 cSt
14.9 cSt
Ash 1.18 %
1.18 %
Sulfated Ash
Thermal Properties Metric English Comments
Pour Point -33.0 °C
-27.4 °F
Flash Point 250 °C
482 °F
Component Elements Properties Metric English Comments
Phosphorous, P 0.114 %
0.114 %
Zinc, Zn 0.127 %
0.127 %
Chemical Properties Metric English Comments
Total Base Number 9.2
9.2
ASTM D2896