China Tungsten WC 97 Tungsten Carbide Powder

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten WC 97 Tungsten Carbide Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Component Elements Properties Metric English Comments
Cobalt, Co 3.0 %
3.0 %
WC 97 %
97 %