Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and designed to be processed using especially adapted physical foam extrusion lines. Supplied as free-foaming pellets in 25 kilogram (55 pound) moisture barrier bags.Features: Fast, easy injection molding, especially for complex part geometriesGood Sealing PerformanceExcellent surface aspectMinimal part warpageCan be injected at lower molding temperatures or at lower injection pressuresLow odorVery low foggingProduct Notes: Values are for injection molded plaques, side gated.82.6 mm x 117.5 mm x 3 mmInformation provided by Advanced Elastomer Systems.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
5 seconds; ASTM D2240
Tensile Strength at Break 8.48 MPa
1230 psi
Across flow; ASTM D412
Tensile Strength, Yield 3.60 MPa

@Strain 100 %
522 psi

@Strain 100 %
across flow; ASTM D412
Elongation at Break 460 %
460 %
Across flow; ASTM D412
Tear Strength 13.0 kN/m
74.0 pli
212°F; ASTM D624
28.0 kN/m
160 pli
73°F; ASTM D624
Compression Set 24 %
24 %
73°F, 170 hr; ASTM D395
38 %
38 %
212°F, 170 hr; ASTM D395
Tensile Set 14 %
14 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Continuously for 1000 hours
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Processing Properties Metric English Comments
Drying Temperature 82.0 °C
180 °F
Desiccant Dryer
Dry Time 3 hour
3 hour
Desiccant Dryer
Users viewing this material also viewed the following: