China Tungsten Z20 Tungsten Carbide for Mining Purposes

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten Z20 Tungsten Carbide for Mining Purposes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent wear resistance and toughness, for pillar bit drills.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.65 - 14.85 g/cc
0.5293 - 0.5365 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 87.5 - 89
87.5 - 89
Flexural Strength 2100 - 2500 MPa
305000 - 363000 psi