Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2100 - 2500 MPa | 305000 - 363000 psi | |
China Tungsten Z20 Tungsten Carbide for Mining Purposes Excellent wear resistance and toughness, for pillar bit drills.Information provided by China Tungsten |