Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
0.007848 GPa

@Temperature 500 °C,
Time 10800 sec
1.138 ksi

@Temperature 932 °F,
Time 3.00 hour
Compressive Strength 11.8 MPa

@Temperature 110 °C,
Time 86400 sec
1710 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
17.7 MPa

@Temperature 500 °C,
Time 10800 sec
2560 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 500 °C
932 °F
limited
Shrinkage -0.200 %

@Temperature 110 °C,
Time 86400 sec
-0.200 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 31 %
31 %
SiO2 62 %
62 %
Descriptive Properties Value Comments
Installation Method Spray
Main Applications Chemical Plant
Material Required for Estimating (kg/?) 2,050