Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 0.9960 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories A64 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories APC-100G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 500 °C,
Time 10800 sec
0.9960 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories APC-120G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories APC-50G Acid-proof Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1400 °C
0.9960 ksi

@Temperature 2550 °F
Chosun Refractories CRAG-S27 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1400 °C
0.9960 ksi

@Temperature 2550 °F
Chosun Refractories CRAG-S50 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1400 °C
0.9960 ksi

@Temperature 2550 °F
Chosun Refractories CRAG-S50 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 - 0.010791 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 - 1.5651 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HACT-180G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 - 0.010791 GPa

@Temperature 1000 °C,
Time 10800 sec
0.9960 - 1.5651 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HACT-180G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1350 °C,
Time 10800 sec
0.9960 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories LPCT-16DS Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories LPCT-18PI Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories MMCT-75 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SFC-70R High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SW87 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 1500 °C,
Time 10800 sec
0.9960 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories SW88 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories TCH-165Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved