Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.32 g/cc
0.0838 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Compressive Strength 49.0 MPa
7110 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 5.80 µm/m-°C

@Temperature 1000 °C
3.22 µin/in-°F

@Temperature 1830 °F
Shrinkage -0.200 - 0.20 %

@Temperature 1350 °C,
Time 7200 sec
-0.200 - 0.20 %

@Temperature 2460 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 43 %
43 %
Fe2O3 1.5 %
1.5 %
Descriptive Properties Value Comments
Quality Anti-abrasion, Anti-spalling
Refractories Under Load(2kg/?,T2?) 1,450
Refractoriness (SK) 34