Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.32 g/cc | 0.0838 lb/in³ | |
Chosun Refractories CRAG-S04 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.32 g/cc | 0.0838 lb/in³ | |
Chosun Refractories SF34 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.32 g/cc | 0.0838 lb/in³ | |
Chosun Refractories CH-S Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |