Chosun Refractories MSM-38 High-Adhesion Mortar

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories MSM-38 High-Adhesion Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Grain Size 75 µm
75 µm
50% <= 0.075 mm
500 µm
500 µm
2% >= 0.50 mm
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
6.867 MPa

@Temperature 1400 °C,
Time 10800 sec
996.0 psi

@Temperature 2550 °F,
Time 3.00 hour
Descriptive Properties Value Comments
Chemical Analysis(%) 80=, 2=
Main Applications Phosphate bond Mortar
Refractoriness (SK),Al2O3,Fe2O3 38=