Physical Properties Metric English Comments
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories AMCM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories AMCM-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories ASCM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories ASCM-S Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories BM-2W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories BM-3W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories GM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
1% >= 0.50 mm
Chosun Refractories HM-A Special Mortar for Sliding Gate Valve
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories HM-B(HM-4AG) Special Mortar for Sliding Gate Valve
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories MSM-36 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories MSM-38 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories MSM-39 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories MSM-40 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories RAPN Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SCH-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SP-3000 High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SP-3000S High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SP-60W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SP-70W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SP-85W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories SP-85W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories BM-1W High-Adhesion Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Grain Size 500 µm
500 µm
2% >= 0.50 mm
Chosun Refractories WM-SN Special Mortar for Sliding Gate Valve
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).