Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Compressive Strength 73.5 MPa

@Temperature 110 °C,
Time 86400 sec
10700 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
108 MPa

@Temperature 1400 °C,
Time 10800 sec
15600 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -0.200 %

@Temperature 1400 °C,
Time 10800 sec
-0.200 %

@Temperature 2550 °F,
Time 3.00 hour
0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 17 %
17 %
SiC 50 %
50 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Material Required for Estimating (kg/?) 2,400
Water Required for Casting(%) 7.5