Polymer Property : Compressive Strength = 73.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 73.5 MPa

@Temperature 110 °C
10700 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC45 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 73.5 MPa

@Temperature 1100 °C
10700 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 006 Smart Cast Application
Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength >= 73.5 MPa

@Temperature 110 °C
>= 10700 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics VELCRETE G 401 Gunning Castables
Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling ..
Compressive Strength 73.5 MPa

@Temperature 1100 °C
10700 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 012 Smart Cast Application
Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn..
Compressive Strength 73.5 MPa

@Temperature 1350 °C,
Time 10800 sec
10700 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MMCT-95 Special Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 73.5 MPa

@Temperature 110 °C,
Time 86400 sec
10700 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SCX-50KL Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).