Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC

Category Ceramic , Carbide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.66 g/cc
0.0961 lb/in³
Porosity 14 %
14 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.04905 GPa

@Temperature 250 °C
7.114 ksi

@Temperature 482 °F
0.04905 GPa

@Temperature 1400 °C
7.114 ksi

@Temperature 2550 °F
Compressive Strength 196 MPa
28400 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C

@Temperature 1000 °C
2.44 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Fe2O3 0.30 %
0.30 %
SiC 95 %
95 %
Descriptive Properties Value Comments
Refractories Under Load(2kg/?,T2?) 1,700<