Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.04905 GPa @Temperature 250 °C |
7.114 ksi @Temperature 482 °F |
|
Chosun Refractories SBN-1 Bricks, Reaction Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.04905 GPa @Temperature 1400 °C |
7.114 ksi @Temperature 2550 °F |
|
Chosun Refractories SBN-1 Bricks, Reaction Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.04905 GPa @Temperature 250 °C |
7.114 ksi @Temperature 482 °F |
|
Chosun Refractories SBSN-CT Tube Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.04905 GPa @Temperature 250 °C |
7.114 ksi @Temperature 482 °F |
|
Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.04905 GPa @Temperature 1400 °C |
7.114 ksi @Temperature 2550 °F |
|
Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.04905 GPa @Temperature 250 °C |
7.114 ksi @Temperature 482 °F |
|
Chosun Refractories SSBN Tube Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |