Clariant Renol ABNN732017 Nylon 6 with anchored silicone

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol ABNN732017 Nylon 6 with anchored silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.98 MPa
5509 psi
ASTM D638
Tensile Strength, Yield 81.4 MPa
11800 psi
ASTM D638
Elongation at Break 19 %
19 %
ASTM D638
Elongation at Yield 7.5 %
7.5 %
ASTM D638
Tensile Modulus 1.50 GPa
217 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Temperature 22.8 °C
1.40 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Coefficient of Friction 0.10
0.10
ASTM D3702
0.17
0.17
ASTM D3702
Processing Properties Metric English Comments
Melt Temperature 210 - 240 °C
410 - 464 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Dry Time 2 - 4 hour
2 - 4 hour
predrying