Material Notes:
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame retardance, low temperature, or chemical resistance, are all available. Formulations for exterior or interior use.Typical Applications: Suction CupsInformation provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 sec; ASTM D2240
Tensile Strength, Ultimate 15.9 MPa
2300 psi
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
100% Modulus 0.00621 GPa
0.900 ksi
ASTM D638