Compuestos Dominicanos Polycom PT-109599 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Compuestos Dominicanos, S.A. (polycom)
Trade Name Polycom
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Compuestos Dominicanos Polycom PT-109599 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polycom rigid PVC compounds for the extrusion of pipes have excellent processing characteristics and are available in the form of pellets and dry blend. They are available with lead and tin stabilizer systems. Compuestos Dominicanos also produces compounds for the injection molding of pipefitting, having outstanding characteristics of flow and impact resistance, being suitable for the production of both drainage and pressure fittings and accessories. The polycom PW series are compounds for the extrusion of window profiles, yielding profiles with superior gloss, color uniformity and impact resistance.Application: PipesAppearance: White pellets or dry blend. Lead stabilizer systemInformation provided by Compuestos Dominicanos, S.A.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.43 g/cc
1.39 - 1.43 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.6 MPa
7200 psi
ASTM D412
Izod Impact, Unnotched 0.392 J/cm
0.735 ft-lb/in
ASTM D256-93