ConocoPhillips 46 FC Fluid-D ISO

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips 46 FC Fluid-D ISO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco FC Fluid-D is a premixed, ready-to-use fluid for hydraulic systems, such as those found in underground-mining equipment that operate where fire-hazard and other personnel safety concerns require water content for fire control. It is typically used in hydraulic systems that operate at pressures as high as 2,000 psi, including die-casting services, steel mills, underground mining and power transmissions. It is approved by the Factory Mutual Research Corporation (FMRC) as a Group I hydraulic fluid and meets U.S. Steel Requirement #171. It is dyed red for easy leak detection. FC Fluid-D does not contain nitrites and, therefore, cannot form nitrosoamines. To prevent water loss, it should not be used where hydraulic sump temperatures exceed 150°F. To maintain adequate fire resistance, water content should not be allowed to drop below 30 percent by volume. Only distilled, deionized or controlled boiler feedwaters should be used for makeup. Filters, seals, packing, gaskets, pipe-joint compounds, paints and metals must be compatible with glycol/water fluids. Filters 25 micron and smaller have been used successfully in systems using FC Fluid-D. Use Viton, EPDM, silicone, butyl, Buna N or neoprene seals; avoid cork and leather. Compatible metals include copper, brass, iron (cast) and steel. Aluminum is not compatible. Glycol/water fluids should not be used in systems that include solder, tin, lead, magnesium, zinc, galvanized piping or cadmium, since the fluids will corrode these metals. Glycol/water fluids are incompatible with conventional industrial paints; use special paints and coatings. Has no fire or flash point.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
pH 9.0
9.0
at 77°F
Viscosity Measurement 185
185
Viscosity Index
Saybolt Viscosity at 100°F 198 SUS
198 SUS
Kinematic Viscosity at 40°C (104°F) 42 cSt
42 cSt
Mechanical Properties Metric English Comments
Four Ball Wear 0.540 mm
0.0213 in
40 kg. 1200 rpm, 1- hr at 167°F
0.660 mm
0.0260 in
40 kg. 1800 rpm, 1- hr at 130°F
Thermal Properties Metric English Comments
Melting Point -47.2 °C
-53.0 °F
Freezing point
Boiling Point 104 °C
219 °F
Descriptive Properties Value Comments
ASTM Rust Test A Pass
Color Red
Vickers 104°C Pump Test 20
150°F, 2000 psi, 100-Hrs. Vane wear (mg.)
Vickers 104°C Pump Test (modified) 20
2000 psi, 10 gpm, 150°F, 1200 rpm, 100-Hrs. Vane wear (mg.)
Water Content 39 wt. %
Users viewing this material also viewed the following: