Polymer Property : Four Ball Wear = 0.540 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.540 mm
0.0213 in
ELM® White Lithium Biodegradable Lubricating Grease
Description: White Lithium Grease is premium quality biodegradable, Biotechbased™ multipurpose grease formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed f..
Four Ball Wear 0.540 mm
0.0213 in
40 kg. 1200 rpm, 1- hr at 167°F
ConocoPhillips 46 FC Fluid-D ISO
Description: Conoco FC Fluid-D is a premixed, ready-to-use fluid for hydraulic systems, such as those found in underground-mining equipment that operate where fire-hazard and other personnel safety ..