ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer ConocoPhillips
Trade Name ANDEROL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep valves clean. FGC 150 meets the former H-1 approval requirements of the USDA where incidental food contact can occur. It is specifically recommended for use in reciprocating compressors where incidental food contact may occur with oil in the discharge air. ANDEROL food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.” The Islamic Food and Nutrition Council of America (IFANCA) endorses FGC 150 Fluid as being produced in conformity with all requirements of Halal.Information provided by ConocoPhillips.Anderol® is a registered trademark of The Anderol Company.
Physical Properties Metric English Comments
Specific Gravity 0.850 g/cc
0.850 g/cc
60°F; ASTM D-1298
Saybolt Viscosity at 100°F 737 SUS
737 SUS
ASTM D-2161
Saybolt Viscosity at 210°F 99 SUS
99 SUS
ASTM D-2161
Kinematic Viscosity at 40°C (104°F) 158 cSt
158 cSt
ASTM D-445
Kinematic Viscosity at 100°C (212°F) 20 cSt
20 cSt
ASTM D-445
Mechanical Properties Metric English Comments
Four Ball Wear 0.600 mm
0.0236 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
Thermal Properties Metric English Comments
Pour Point -35.0 °C
-31.0 °F
ASTM D-97
Flash Point 250 °C
482 °F
ASTM D-92
Descriptive Properties Value Comments
Copper Corrosion 1A
3 hrs. at 100°C, ASTM D130
Demulsibility (40-40-0) Max 30 minutes
at 54°C, ml oil/water/emulsion, ASTM D1401
Evaporation Max 1.0 %
ASTM D-972, 22 hrs. @ 99°C (210°F)