Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 158 cSt | 158 cSt | Base Oil; ASTM D445 |
Nye Lubricants 148 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 158 cSt | 158 cSt | ASTM D445 |
ExxonMobil Mobil Rarus 829 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Kinematic Viscosity at 40°C (104°F) | 158 cSt | 158 cSt | ASTM D445 |
ExxonMobil Mobil Rarus 829 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Kinematic Viscosity at 40°C (104°F) | 158 cSt | 158 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150 Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val.. |
|||
Kinematic Viscosity at 40°C (104°F) | 158 cSt | 158 cSt | Base Oil |
ConocoPhillips EP Conolith® HT Grease NLGI NO.2 Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wh.. |