ConocoPhillips Conoco® El Mar® 15W-40 Mid Ash Heavy Duty

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Conoco® El Mar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Conoco® El Mar® 15W-40 Mid Ash Heavy Duty.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natural gas engines. It is particularly recommended for use in natural gas engines and dual-fuel engines burning sour gas or landfill gas. El Mar Mid Ash Heavy Duty is formulated with field-proven performance additives to provide excellent resistance to oxidation and nitration, protect against piston scuffing and wear, and minimize the formation of sludge and piston deposits for good engine cleanliness. It has a high alkaline reserve (TBN) to protect engines operating under corrosive conditions, such as when burning sour gas, digester gas or landfill gas.Applications: 4-stroke cycle gas and dual-fuel engines burning sour gas or landfill gas 4-stroke cycle natural gas engines in wastewater treatment plants fueled by digester gas 4-stroke cycle converted irrigation engines running on natural gas or LPG Other 4-stroke cycle natural gas engines where the manufacturer specifies a mid-ash gas engine oil El Mar Mid Ash Heavy Duty is recommended for use in natural gas engines manufactured by: Cooper Superior Waukesha (VHP GL turbocharged lean-burn engines, models 3521, 5115, 7042, 9390Features/Benefit: Excellent resistance to oxidation and nitration High alkaline reserve to combat acidic combustion by-products when burning sour gas High dispersancy protects against sludge and varnish formation Protects against scuffing and wear Protects against rust and corrosion Excellent low-temperature performance Does not contain any bright stock, which can cause harmful carbon depositsInformation provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 0.877 g/cc
0.877 g/cc
Density 0.875 g/cc
0.0316 lb/in³
Viscosity 6300 cP

@Temperature -20.0 °C
6300 cP

@Temperature -4.00 °F
Cold Cranking
Viscosity Measurement 134
134
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 114 cSt
114 cSt
Kinematic Viscosity at 100°C (212°F) 14.8 cSt
14.8 cSt
Ash 1.0 %
1.0 %
Sulfated Ash; ASTM D874
ASTM Color 3.0
3.0
ASTM D1500
Thermal Properties Metric English Comments
Pour Point -45.0 °C
-49.0 °F
Flash Point 232 °C
450 °F
COC
Component Elements Properties Metric English Comments
Phosphorous, P 0.097 %
0.097 %
Zinc, Zn 0.109 %
0.109 %
Chemical Properties Metric English Comments
Total Base Number 7.9
7.9
ASTM D2896
Descriptive Properties Value Comments
Phosphorus 1140 ppm
Zinc 1270 ppm