Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Pyrotek Firefly 800 Roller & Furnace Cladding Material Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Pyrotek U-1 Compressible Board U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo.. |
|||
Density | 0.875 - 2.24 g/cc | 0.0316 - 0.0809 lb/in³ | Average value: 1.11 g/cc Grade Count:307 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D1475 |
Humiseal 1B12 Acrylic Conformal Coating Humiseal 1B12 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityPasses thermal shock test (MIL-I-46058C)Flammabili.. |
|||
Density | 0.875 - 0.899 g/cc | 0.0316 - 0.0325 lb/in³ | |
Lord Adhesives 7707 n-Butyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.875 g/cc @Temperature 20.0 °C |
0.0316 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PNB Propylene glycol normal butyl ether Information provided by Lyondell. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Silon Tabond 3042 Impact Modifier for PA Tabond 3042 is a chemically modified Ethylene Copolymer/LLDPE.Information provided by Silon |
|||
Density | 0.875 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 75W-80 Mobilfluid LT Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to.. |
|||
Density | 0.875 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Dow AFFINITY™ KC 8852 Polyolefin Elastomer AFFINITY® KC 8852 polyolefin elastomer is an ethylene-octene copolymer as for one sided stretch cling film in industrial collation packaging. It exhibits excellent inherent cling and optics while o.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D792 |
Dow AFFINITY™ KC 8852G Polyolefin Plastomer (POP) AFFINITY™ KC 8852G is an ethylene-octene copolymer produced via INSITE™ Technology. This product offers excellent performance as a cling resin in one-sided stretch cling film applications. This .. |
|||
Density | 0.875 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 75W-80 Mobilfluid LT Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D792 |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Density | 0.875 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® 150 Circulating Oil Description: Conoco Hydroclear Circulating Oil is a high-quality, rust-inhibited circulating oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Circulating Oil is specially form.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
ConocoPhillips 100M Gear Oil AGMA Lubricant No. 3EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Density | 0.875 g/cc @Temperature 20.0 °C |
0.0316 lb/in³ @Temperature 68.0 °F |
|
Akzo Nobel Trigonox® 301 Polymerization Initiator Initiator for the production of controlled rheology polypropylene (CR-PP).Chemical description: 3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane, 41% solution in isoparaffinic hydrocarbonsCAS Numb.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
3M Hi-Strength 90 Spray Adhesive-Low VOC An industrial grade high strength aerosol spray adhesive.Features:Bonds to a variety of substrates including decorative laminate, headliners, and soft foams.Typically used in construction, woodworki.. |
|||
Density | 0.875 g/cc @Temperature 0.000 °C |
0.0316 lb/in³ @Temperature 32.0 °F |
|
BorsodChem ONGRONOX INP 75 D peroxide-type initiator Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide.Mol. wt: 314.50 g/mol.Active oxygen content: 5.09 %.Deflegmation material: isododecane.Major decomposition products.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Conoco® El Mar® 15W-40 Mid Ash Heavy Duty Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Density | 0.875 g/cc @Temperature 20.0 °C |
0.0316 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PTB Propylene glycol tertiary butyl ether Information provided by Lyondell. |