ConocoPhillips El Mar® 3000 Oil SAE Grade 40

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name El Mar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips El Mar® 3000 Oil SAE Grade 40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such as Caterpillar*; Cooper-Superior (formerly White-Superior); Waukesha; Navistar (formerly International Harvester); Dresser-Rand (formerly Ingersoll-Rand) Category I, II and III; Minneapolis Moline; Onan and Detroit Diesel (gas or dual-fuel conversion). El Mar 3000 Oil is formulated with high-viscosity index base oils blended with selected additives and a unique ashless dispersant to provide good resistance to oxidation and nitration, reduced carbon-forming tendencies, good piston ring groove and crankcase cleanliness and ring and liner protection. Highly loaded engines (>80 percent) and/or engines operated with extended lubricant drain intervals may build engine deposits, which may become excessive. If operating under these extreme conditions, Hydroclear El Mar LA4 is recommended. Remote engines operated intermittently or in cold weather benefit from the low temperature pumpability provided by the SAE 15W-40 viscosity grade.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 0.884 g/cc
0.884 g/cc
60°F
Density 0.882 g/cc
0.0319 lb/in³
API Gravity 28.6 °
28.6 °
Viscosity Measurement 93
93
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 124 cSt
124 cSt
Kinematic Viscosity at 100°C (212°F) 13 cSt
13 cSt
Ash 0.41 %
0.41 %
Sulfated Ash
ASTM Color 3.5
3.5
Thermal Properties Metric English Comments
Pour Point -8.89 °C
16.0 °F
Flash Point 257 °C
495 °F
Chemical Properties Metric English Comments
Total Base Number 5.1
5.1