Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 257 °C | 495 °F | |
Lubriplate FMO 500 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Flash Point | 257 °C | 495 °F | |
Lubriplate RCO 68 PAO-Based Synthetic Food Machinery Grade Fluid Formulated for use in refrigeration compressor systems where a NSF H-1 Registered, food machinery grade lubricant is required.RCO-68 Fluid is available in Pails & Drums.H-1 Class Lubricants are manu.. |
|||
Flash Point | 257 °C | 495 °F | |
Lubriplate SFGO Ultra-68 PAO-Based Synthetic Food Machinery Grade Fluid Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi.. |
|||
Flash Point | 257 °C | 495 °F | ASTM D92 |
ExxonMobil Mobil Vaculine 1419 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Flash Point | 257 °C | 495 °F | COC; ASTM D92 |
ExxonMobil Exterex™ NP343 Synthetic Fluid Product Description: Esterex™ Polyol Esters are API category Group V fluids. Esterex™ Polyol Esters have excellent lower-temperature properties, good lubricating properties and low volatilities. E.. |
|||
Flash Point | 257 °C | 495 °F | ASTM D92 |
ExxonMobil Mobil Vaculine 1419 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Flash Point | 257 °C | 495 °F | |
ConocoPhillips El Mar® 3000 Oil SAE Grade 40 Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such.. |