ConocoPhillips Hydroclear® XHP 2-Cycle Engine Oil

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® XHP 2-Cycle Engine Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear XHP 2-Cycle Engine Oil is made with an advanced, high-stability base oil and highly effective additives. This unique combination allows the product to meet full NMMA TC-W3 standards for watercraft engines, “Category 4” standards for SAE gasoline Miscibility/Fluidity and the JASO FB level of performance for air-cooled and water-cooled, land-based engines. Hydroclear XHP 2-Cycle Engine Oil provides maximum protection for marine outboard 2-cycle engines. Its high degree of detergency and dispersancy resists formation of exhaust port deposits, spark plug fouling, ring sticking, piston deposits and piston seizure. Hydroclear XHP 2-Cycle Engine Oil is exceptionally soluble in gasolines and is designed for use with either “direct injection” or “premix” engines.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc
0.870 g/cc
15°C
Density 0.872 g/cc

@Temperature 15.6 °C
0.0315 lb/in³

@Temperature 60.0 °F
Brookfield Viscosity 16600 cP

@Temperature -40.0 °C
16600 cP

@Temperature -40.0 °F
Kinematic Viscosity at 40°C (104°F) 25.5 cSt
25.5 cSt
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
Thermal Properties Metric English Comments
Pour Point -53.9 °C
-65.0 °F
Flash Point 95.0 °C
203 °F
Descriptive Properties Value Comments
Color Blue-Green