Polymer Property : Kinematic Viscosity at 100°C (212°F) = 5.1 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8120 (473) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8122 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 5.1 cSt

@Temperature 100 °C
5.1 cSt

@Temperature 212 °F
ASTM D445
PolyOne Synplast™ DUP-E Di Undecyl Phthalate
Linear C11 phthalate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Aero HF
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Aero HFA
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Jet Oil II
Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combina..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobiltherm 43
Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems.  It has a high specific heat an..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ChevronTexaco 5606G Aircraft Hydraulic Oil
Texaco Aircraft Hydraulic Oil 5606G delivers value through:Minimum viscosity change over a range of operating temperaturesLow pour point which permits operation at the lowest temperatures generally ..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ChevronTexaco Rando® HDZ 22
Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil SpectraSyn™ 5 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) ..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobiltherm 43
Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems.  It has a high specific heat an..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ChevronTexaco Aviation G Hydraulic Fluid
FeaturesChevron Aviation Hydraulic Fluids are both manufactured from specially selected, highly refined, low viscosity and low pour point petroleum base stocks. They both contain a superior, shear ..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Pyrogard 53
Mobil Pyrogard 53 is a high performance phosphate ester synthetic fluid designed to replace petroleum-based oils in hydraulic applications where operating conditions preclude the use of combustible ..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ConocoPhillips Hydroclear® XHP 2-Cycle Engine Oil
Description: Conoco Hydroclear XHP 2-Cycle Engine Oil is made with an advanced, high-stability base oil and highly effective additives. This unique combination allows the product to meet full NMMA T..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Aero HF
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Aero HFA
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Jet Oil II
Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combina..
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
5.1 cSt
ASTM D445
ExxonMobil Mobil Pyrogard 53
Mobil Pyrogard 53 is a high performance phosphate ester synthetic fluid designed to replace petroleum-based oils in hydraulic applications where operating conditions preclude the use of combustible ..