Material Notes:
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.
Physical Properties Metric English Comments
Density 2.64 g/cc
0.0954 lb/in³
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C

@Temperature 0.000 - 300 °C
2.44 µin/in-°F

@Temperature 32.0 - 572 °F
Softening Point 926 °C
1700 °F
Annealing Point 726 °C
1340 °F
Strain Point 674 °C
1250 °F