Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.28 - 1.32 g/cc
1.28 - 1.32 g/cc
ASTM D 792
ASTM Color -1.66 - -0.060
-1.66 - -0.060
Color B, ME 12
-0.810 - 0.79
-0.810 - 0.79
Color A, ME 12
27.46 - 29.06
27.46 - 29.06
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 48 - 52

@Time 15.0 sec
48 - 52

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Thermal Properties Metric English Comments
Brittleness Temperature <= -45.0 °C
<= -49.0 °F
ASTM D 746
Descriptive Properties Value Comments
Application General Purpose Injection Molded Parts