Material Notes:
Crushed/Powdered glass available in mesh sizes 4 through 325 and can be customized. Used primarily as a Kovar Sealing Glass. This product is used in MOEMS applications. Information provided by Corning Incorporated.
Physical Properties Metric English Comments
Density 2.29 g/cc
0.0827 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 62.8 GPa
9110 ksi
Poissons Ratio 0.21
0.21
Shear Modulus 26.5 GPa
3840 ksi
Thermal Properties Metric English Comments
CTE, linear 5.15 µm/m-°C

@Temperature 0.000 - 300 °C
2.86 µin/in-°F

@Temperature 32.0 - 572 °F
5.45 µm/m-°C

@Temperature 25.0 - 679 °C
3.03 µin/in-°F

@Temperature 77.0 - 1250 °F
Set Point
Softening Point 718 °C
1320 °F
10<sup>7.6</sup> Poise
Working Point 1058 °C
1936 °F
10<sup>4</sup> Poise
Annealing Point 512 °C
954 °F
10<sup>13</sup> Poise
Strain Point 472 °C
882 °F
10<sup>14</sup> Poise
Optical Properties Metric English Comments
Refractive Index 1.487

@Wavelength 589.3 nm
1.487

@Wavelength 589.3 nm
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+8 ohm-cm

@Temperature 350 °C
2.50e+8 ohm-cm

@Temperature 662 °F
2.00e+10 ohm-cm

@Temperature 250 °C
2.00e+10 ohm-cm

@Temperature 482 °F
Dielectric Constant 5.7

@Frequency 1e+6 Hz
5.7

@Frequency 1e+6 Hz
Dissipation Factor 0.0027

@Frequency 1e+6 Hz
0.0027

@Frequency 1e+6 Hz