Thermal Properties Metric English Comments
Working Point 1058 °C
1936 °F
10<sup>4</sup> Poise
Corning 7056 Alkali Borosilicate Crushed/Powdered Glass
Crushed/Powdered glass available in mesh sizes 4 through 325 and can be customized. Used primarily as a Kovar Sealing Glass. This product is used in MOEMS applications. Information provided by Corn..