Material Notes:
Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required.
Physical Properties Metric English Comments
Density 3.80 g/cc
0.137 lb/in³
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Viscosity 15000 cP
15000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Tensile Strength, Ultimate 44.8 MPa
6500 psi
Elongation at Break 0.20 %
0.20 %
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 20.0 °C
30.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 7.20 W/m-K
50.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Shrinkage 0.20 %
0.20 %
Electrical Properties Metric English Comments
Volume Resistivity 0.000080 ohm-cm
0.000080 ohm-cm
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 121 °C
0.333 hour

@Temperature 250 °F