Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Covestro
Trade Name Bayfill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.0960 g/cc
0.00347 lb/in³
Molded density, ASTM D3574-A
Apparent Bulk Density 0.0720 g/cc
0.00260 lb/in³
Free-rise Density, Bayer test
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.270 MPa
39.2 psi
ASTM D3574E
Elongation at Break 52 %
52 %
ASTM D3574E
Compressive Yield Strength 0.0440 MPa
6.38 psi
50% Compression, ASTM D3574-D
Tear Strength 0.300 kN/m
1.71 pli
Split Tear Strength, ASTM D3574-F
Compression Set 54 %
54 %
Test C, ASTM D3574 Dry