Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.0720 g/cc | 0.00260 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Apparent Bulk Density | 0.0720 g/cc | 0.00260 lb/in³ | Free-rise Density, Bayer test |
Covestro Bayfill® 361 Polyurethane Semi-Rigid Foam, Conventional Catalyst, Open Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |