Covestro Desmopan® DP 8715 Polyurethane + ABS

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyurethane Alloy , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 8715 Polyurethane + ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding grademodified with ABSgood low-temperature flexibilitygood wear resistanceApplicationSki boot shellsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
3s; ISO 868
Hardness, Shore D 58
58
15s; ISO 868
Tensile Strength at Break 63.0 MPa
9140 psi
ISO 527-1/-2
Tensile Strength, Yield 63.0 MPa
9140 psi
parallel; ISO 527-3
20.0 MPa

@Strain 100 %
2900 psi

@Strain 100 %
ISO 527-1/-2
38.0 MPa

@Strain 300 %
5510 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 25
25
mm³; ISO 4649
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America