Material Notes:
CPM REX 121 is a new high vanadium cobalt bearing tool steel designed to offer a combination of the highest wear resistance, attainable hardness, and red hardness available in a high speed steel. Its superior red hardness permits higher cutting speeds compared to other high speed steels. Its superior wear resistance (due to the high vanadium content) helps maintain a sharp cutting edge at increased cutting speeds.CPM REX 121 also bridges the performance gap between high alloy tool steels and carbide materials. It may be used in cutting tools, where high cutting speeds demand higher heat resistance, but carbide is too brittle, or in high wear tooling applications (punches and dies) where carbide tools are too fragile.Because of the extremely fine and uniform CPM microstructure, sulfur may be added if desired, to improve the machinability. The higher sulfur content benefits the toolmaker by allowing ease of manufacture, and the tool user by allowing easier resharpening. The CPM process ensures that the additional sulfur will not detrimentally affect the tool’s toughness.Information provided by Crucible Industries
Mechanical Properties Metric English Comments
Hardness, Brinell 360 - 410
360 - 410
Hardness, Rockwell C 71
71
hardened at 1875°F
55

@Tempering Temp. 649 °C
55

@Tempering Temp. 1200 °F
hardened at 1875°F then tempered
63

@Tempering Temp. 593 °C
63

@Tempering Temp. 1100 °F
hardened at 1875°F then tempered
66.5

@Tempering Temp. 566 °C
66.5

@Tempering Temp. 1050 °F
hardened at 1875°F then tempered
67.5

@Tempering Temp. 551.7 °C
67.5

@Tempering Temp. 1025 °F
hardened at 1875°F then tempered
68.5

@Tempering Temp. 538 °C
68.5

@Tempering Temp. 1000 °F
hardened at 1875°F then tempered
69

@Tempering Temp. 510 °C
69

@Tempering Temp. 950 °F
hardened at 1875°F then tempered
Modulus of Elasticity 214 GPa
31000 ksi
Component Elements Properties Metric English Comments
Carbon, C 3.4 %
3.4 %
Chromium, Cr 4.0 %
4.0 %
Cobalt, Co 9.0 %
9.0 %
Iron, Fe 59 %
59 %
as balance
Molybdenum, Mo 5.0 %
5.0 %
Sulfur, S 0.030 %
0.030 %
Tungsten, W 10 %
10 %
Vanadium, V 9.5 %
9.5 %
Users viewing this material also viewed the following: