35% Glass Reinforced
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
dry; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 150 MPa
21800 psi
dry; ISO 527-1/-2
Elongation at Break 2.1 %
2.1 %
dry; ISO 527-1/-2
Tensile Modulus 11.3 GPa
1640 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.10 J/cm²

@Temperature 23.0 °C
29.0 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3