Material Notes:
Antisqueak Blow Molding Grade
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 0.70 %
0.70 %
Sim. To ISO 62
Moisture Absorption 0.300 %
0.300 %
Sim. To ISO 62
Melt Flow 6.5 g/10 min

@Load 10.0 kg,
Temperature 230 °C
6.5 g/10 min

@Load 22.0 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 37
37
ISO 868
Tensile Strength, Ultimate 21.0 MPa
3050 psi
ISO 527-1/-2
Tensile Stress 3.50 MPa

@Strain 5.00 %
508 psi

@Strain 5.00 %
ISO 527-1/-2
6.00 MPa

@Strain 10.0 %
870 psi

@Strain 10.0 %
ISO 527-1/-2
11.2 MPa

@Strain 50.0 %
1620 psi

@Strain 50.0 %
ISO 527-1/-2
14.0 MPa

@Strain 100 %
2030 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 275 %
275 %
ISO 527-1/-2
Tensile Modulus 0.0650 GPa
9.43 ksi
ISO 527-1/-2
Izod Impact Resistance NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 214 °C
417 °F
10°C/min; ISO 11357-1/-3