DSM Stanyl® TS271A1 PA46-RF

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TS271A1 PA46-RF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aramid fiber reinforced, Wear and Friction Modified
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
dry; ISO 1183
Moisture Absorption 2.90 %
2.90 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
dry; ISO 527-1/-2
Elongation at Break 13 %
13 %
dry; ISO 527-1/-2
Tensile Modulus 2.80 GPa
406 ksi
dry; ISO 527-1/-2
Flexural Modulus 3.10 GPa
450 ksi
dry; ISO 178
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
dry; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
dry; IEC 60695-11-10