Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Daikin NEOFLON NC-1810 FEP Coating Powder, White

Category Polymer , Thermoplastic , Fluoropolymer , FEP , Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Manufacturer Daikin Industries
Trade Name NEOFLON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Daikin NEOFLON NC-1810 FEP Coating Powder, White.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
Oxygen Transmission 320 cc-mm/m²-24hr-atm
812 cc-mil/100 in²-24hr-atm
at 25°C
Nitrogen Transmission 104 cc-mm/m²-24hr-atm
263 cc-mil/100 in²-24hr-atm
at 25°C
Thickness 500 - 5000 microns
19.7 - 197 mil
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
FEP Component
Oxygen Index >= 95 %
>= 95 %
FEP Component
Electrical Properties Metric English Comments
Dielectric Constant 2.0 - 2.2

@Frequency 1000 Hz
2.0 - 2.2

@Frequency 1000 Hz
FEP Component; ASTM D150
2.0 - 2.2

@Frequency 1e+6 Hz
2.0 - 2.2

@Frequency 1e+6 Hz
FEP Component; ASTM D150
Dissipation Factor 0.00010 - 0.00030
0.00010 - 0.00030
FEP Component
Users viewing this material also viewed the following: