Daikin POLYFLON L-5F PTFE Low Polymer, White Fine Powder

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Daikin Industries
Trade Name POLYFLON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Daikin POLYFLON L-5F PTFE Low Polymer, White Fine Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White fine powder.Major Uses: Extreme pressure additive and lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, etc.Information provided by Daikin Industries.
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc
2.20 g/cc
Bulk Density 0.420 g/cc
0.0152 lb/in³
Particle Size 5.0 µm
5.0 µm
Average
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
PTFE Component
Oxygen Index >= 95 %
>= 95 %
PTFE Component
Electrical Properties Metric English Comments
Dielectric Constant 2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
PTFE Component; ASTM D150
2.1

@Frequency 1e+6 Hz
2.1

@Frequency 1e+6 Hz
PTFE Component; ASTM D150
Dissipation Factor 0.00010 - 0.00022
0.00010 - 0.00022
PTFE Component