Diamond Polymers DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend, Glass Reinforced , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
14900 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 6.759 GPa
980.3 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Descriptive Properties Value Comments
Glass Content (%) 30
ASTM D5630